In this study, Cu-10% vol. TiC nanocomposites were ball milled and spark plasma sintered for 5 min at 600, 700 and 800 °C under pressure of 50 MPa to produce bulk materials with relative densities of (94.6-96.5) %…
In this study, Cu-10% vol. TiC nanocomposites were ball milled and spark plasma sintered for 5 min at 600, 700 and 800 °C under pressure of 50 MPa to produce bulk materials with relative densities of (94.6-96.5) %…